Morphological observations
samples sensitized at 650°C for 5 h after polarisation in HClO4 1M + 7000 ppm Cl- (1000X)
Microscopic observations showed that intergranular corrosion is the main corrosion phenomenum.
It is worth noticing the great difference, in terms of depth of corrosion attack, between the two samples.