CBA RESULTS: coatings E+I and E+B
The steep decrease of the stress after the maximum is related to the formation of cracks that very rapidly widen and produce the collapse of the coating. The constant value of the stress observable in the first stage of the measurements is ascribable to the slight adjustment of the coated slab after its imposed breaking through bending.
The same behaviour was obtained for coating E+B.